Washing and Curing Resin Prints: IPA, Water-Washable and Cure Times

by | Nov 26, 2026

Wash resin prints in two baths of isopropyl alcohol (IPA), about 2–3 minutes each, or in water if you use water-washable resin. Let the print dry completely, take the supports off while it’s still slightly soft, then cure it under UV light for 2–4 minutes for a 32 mm miniature, turning it so every side gets light. Over-washing and over-curing both make miniatures brittle, so shorter is usually better.

This guide covers washing and curing step by step, with times for typical standard and water-washable resins and the mistakes that cause sticky, cracked or white, chalky prints.

In this guide
  1. Why washing and curing matter
  2. Safety first
  3. Washing: IPA or water?
  4. How to wash, step by step
  5. Removing supports (before curing)
  6. Curing: how long?
  7. Common washing and curing problems
  8. Dealing with dirty IPA and water
  9. Frequently asked questions
  10. Next steps

Why washing and curing matter

A print fresh off the build plate is covered in liquid, uncured resin and is only partly hardened inside.

  • Washing removes the liquid resin. Skip it and you get a sticky surface, lost detail and a skin irritant on your hands.
  • Curing finishes hardening the resin with UV light. Uncured prints stay soft, tacky and are not safe to handle without gloves.

Safety first

Wear nitrile gloves for every step until the print is cured. Liquid resin can cause skin allergies that build up over time. Work with ventilation, keep IPA away from flames (it’s highly flammable), and never pour resin or dirty IPA down the sink. More detail is in the safety section of our resin printing guide.

Washing: IPA or water?

Standard resin + IPA Water-washable resin + water
Cleaning power Very good Good
Cost of washing IPA has to be bought and replaced Cheap
Smell Alcohol smell Mild
Waste Dirty IPA must be cured and disposed of properly Dirty water is still hazardous: cure it the same way, never pour it away
Brittleness Normal Water-washable resins are often a little more brittle

Use 90%+ isopropyl alcohol for standard resin. Lower concentrations clean poorly and leave a white film.

How to wash, step by step

  1. Let the plate drip over the vat for a few minutes so excess resin drains back.
  2. Remove the prints from the plate with the scraper (or wash them on the plate if your wash station takes it).
  3. First bath (the “dirty” tub): 2–3 minutes, swirling or with the wash station’s agitator. This takes off most of the resin.
  4. Second bath (the “clean” tub): 1–2 minutes to remove the last film.
  5. Check recesses like the inside of cloaks and between legs. A soft brush dipped in clean IPA reaches spots the bath missed.
  6. Dry completely. Air dry for 15–30 minutes, or use a fan or a cool hairdryer setting. IPA trapped in recesses turns white and chalky when cured.

Wash time is a balance. Under-washing leaves a tacky film; leaving prints in IPA for 10 minutes or more can make thin parts soft, swollen and prone to cracking.

Removing supports (before curing)

Take supports off after washing and drying but before curing. The resin is still slightly flexible, so supports snap cleanly and tiny details are less likely to break. Clip close with flush cutters rather than twisting. Warm (not hot) water softens supports further. See How to Support Miniatures for Resin Printing for how to place them so removal is easy.

Curing: how long?

Starting points for small miniatures (about 28–32 mm):

Light source Time Notes
Wash-and-cure station (turntable) 2–4 minutes Easiest and most even
UV nail lamp or UV torch 3–5 minutes, turning by hand Make sure every side gets light
Sunlight 15–60 minutes depending on weather Works, but slow and uneven in UK winters

Larger models need longer, roughly 5–10 minutes, and hollow models need light inside too (shine a UV torch into the drain hole).

Signs of under-curing: surface still tacky, soft when pressed with a fingernail, smells strongly of resin. Signs of over-curing: yellowing, brittle parts that snap, fine details cracking.

Cure in short bursts and test. You can always add another minute; you can’t undo over-curing.

Common washing and curing problems

Problem Likely cause Fix
White, chalky residue IPA not dried before curing, or dirty IPA Dry fully before curing; refresh your clean bath
Sticky after curing Not washed enough, or not cured enough Re-wash briefly in clean IPA, then cure another minute or two
Cracks appearing hours later Over-washing or over-curing, or a solid model with trapped resin Shorter wash and cure; hollow larger models with drain holes
Yellow tint Over-curing Shorter cure time
Thin parts bent Soft from too long in IPA, or cured while bent Shorter wash; straighten gently with warm water before curing

Dealing with dirty IPA and water

  1. Leave the dirty IPA or water in a clear container in sunlight (or under a UV lamp) for a day or two. The resin in it cures into solid sludge.
  2. Filter the liquid through a coffee filter or paper towel. Clean IPA can be reused.
  3. The solid resin and filters are hardened waste: bag them and take them to your local household waste recycling centre, or follow your council’s rules.
  4. Never pour uncured resin, dirty IPA or “washing water” down the sink or into the garden.

Frequently asked questions

How long should I wash resin prints in IPA? About 2–3 minutes in a dirty bath and 1–2 minutes in a clean bath. Longer can soften thin parts.

How long do I cure a 32 mm miniature? 2–4 minutes in a cure station, or 3–5 minutes under a lamp while turning it.

Should I remove supports before or after curing? Before. Uncured resin is slightly flexible, so supports come off cleaner.

Why is my print white after curing? Usually IPA left in recesses that wasn’t dried before curing, or a dirty IPA bath. Let prints dry fully and refresh your clean tub.