Most failed resin prints come down to four things: the plate isn’t level or clean, bottom exposure is too low, the resin is too cold, or the model is badly oriented and under-supported. Check those first. Below are the 12 problems we see most often with miniatures, what each one looks like, and how to fix it.
Before you change anything, check the vat film for holes and the vat for cured bits of resin. A tiny cured flake from a failed print will ruin the next one. Run your printer’s “clean vat” or “exposure” function, or gently sweep the film with a plastic scraper.
In this guide
- Quick diagnosis table
- 1. Nothing sticks to the build plate
- 2. The raft printed, but the model didn't
- 3. Missing fingers, sword tips and other small parts
- 4. Layer shift or visible step partway up
- 5. Delamination (the model splits into layers)
- 6. Holes, craters and blow-outs
- 7. Bloated, blobby details
- 8. Soft or bendy parts
- 9. Rough, crusty patches under overhangs
- 10. The raft peels off the plate partway through
- 11. Elephant's foot
- 12. The print cracks days later
- Check this before every print
- Frequently asked questions
- Next steps
Quick diagnosis table
| # | What you see | Most likely cause |
|---|---|---|
| 1 | Nothing on the plate, all on the film | Bottom exposure too low, plate not level, cold resin |
| 2 | Raft on the plate, model missing | Weak supports, too few supports, bad angle |
| 3 | Missing fingers, tips or weapon ends | Missed islands |
| 4 | Layer lines or a “shift” partway up | Loose plate or vat, Z-axis problem |
| 5 | Model split into layers (delamination) | Too much peel force, cold resin, underexposure |
| 6 | Holes, craters or cracks | Suction cups, hollow model without drain holes |
| 7 | Blobby, bloated detail | Overexposure |
| 8 | Soft, rubbery or bendy parts | Underexposure or cold resin |
| 9 | Rough “crusty” bits under overhangs | Missed islands or underexposed supports |
| 10 | Raft peels off the plate partway | Plate dirty or smooth, bottom exposure too low |
| 11 | Elephant’s foot (raft edge flares out) | Bottom layers overexposed |
| 12 | Print fine but cracks days later | Over-curing, trapped resin, over-washing |
1. Nothing sticks to the build plate
Looks like: an empty plate and a sheet of cured resin stuck to the vat film.
Fixes:
- Re-level the plate using your printer’s paper method.
- Clean and lightly sand the plate (fine sandpaper in a cross-hatch) so the raft can grip.
- Raise the bottom exposure by a few seconds, or add 1–2 more bottom layers.
- Warm the room and the resin to at least 20–25 °C. Cold resin is the most common winter failure in the UK.
- Clear the vat of any cured flakes before the next attempt.
2. The raft printed, but the model didn’t
The supports broke and the model fell into the vat.
Fixes: tilt the model 30–45° so layers are smaller, use heavier supports near the base, add more medium supports, and check that support tips aren’t too thin for your resin. See How to Support Miniatures for Resin Printing.
3. Missing fingers, sword tips and other small parts
These parts were islands with no support under them, so they printed into mid-air.
Fix: run your slicer’s island check and scroll through the layers from the bottom up. Add a light support under every new shape that appears.
4. Layer shift or visible step partway up
Fixes: tighten the build plate and vat screws, check that nothing touches the plate as it moves, and clean and lubricate the Z-axis lead screw if your printer’s manual recommends it.
5. Delamination (the model splits into layers)
Layers don’t bond to each other, often showing as a crack across the model.
Fixes: reduce the size of each layer by tilting the model more, raise normal exposure slightly, slow the lift speed, add a “rest time” after lift if your slicer has one, and keep the resin warm.
6. Holes, craters and blow-outs
These come from suction: a cup-shaped area or a hollow model traps resin and creates a vacuum as the plate lifts.
Fixes: reorient the model so no area faces down like a bowl, or add at least two drain holes to hollow models (one for resin out, one for air in). Small 28–32 mm minis are best printed solid.
7. Bloated, blobby details
Fine details look puffy, and gaps between fingers or chainmail fill in.
Fix: lower normal exposure in small steps (0.1–0.2 s). Run your resin’s exposure test print (such as the Cones of Calibration or a resin manufacturer’s test) to find the sweet spot.
8. Soft or bendy parts
Thin parts like spears, bows and tails come out flexible and droop.
Fixes: raise normal exposure slightly, warm the resin, and add supports along long thin parts. Also make sure you’re not leaving prints too long in IPA, which softens them (see Washing and Curing Resin Prints).
9. Rough, crusty patches under overhangs
Fixes: more supports under the overhang, and an island check. If supports themselves are failing, use a slightly thicker tip.
10. The raft peels off the plate partway through
Fixes: clean the plate with IPA, lightly sand it, and add a little bottom exposure. Check the plate is level and that the raft isn’t printed with a huge solid area (a thinner or “skate” style raft helps).
11. Elephant’s foot
The bottom of the raft flares out, making it hard to remove.
Fix: lower bottom exposure a little, or use a raft with a chamfered edge so your scraper slides under it. It only matters for the raft, not the model.
12. The print cracks days later
Causes: over-curing, a solid large model with liquid resin trapped inside, or prints left in IPA too long.
Fixes: shorter cure times (2–4 minutes for small minis), hollow and drain larger models, and keep washes short.
Check this before every print
- Resin shaken and warm (20–25 °C).
- Vat clean, film undamaged, resin topped up.
- Plate clean and level.
- Model tilted 30–45°, supported, island-checked.
- Exposure set from a recent test for this resin.
Frequently asked questions
Why do my resin prints fail in winter? Cold resin is thicker and cures less well. Keep the room and resin at 20–25 °C. Some people use a small enclosure heater made for resin printers.
What’s the best first fix for a failed print? Clean the vat, check the film, re-level the plate and warm the resin. These fix most failures before you touch any settings.
How do I find the right exposure? Print an exposure test (most resin makers and slicers offer one) and adjust in small steps.
My print stuck to the film. Is the film ruined? Not usually. Gently remove the cured layer with a plastic scraper, check the film against a light for holes, and filter the resin before printing again.